Home   /   Thesis   /   Phenomenological study of the coupled effects of iodine and oxygen on Iodine induced Stress-Corrosion-Cracking (I-SCC) of zirconium alloys

Phenomenological study of the coupled effects of iodine and oxygen on Iodine induced Stress-Corrosion-Cracking (I-SCC) of zirconium alloys

Engineering sciences Materials and applications

Abstract

The Pressurized Water Reactor (PWR) core is composed of fuel assemblies, for which the fuel cladding is the first barrier for the confinement of the fuel and the fission products. Pellet Cladding Interaction (PCI) occurs during increases in the reactor power and results in the expansion of the pellets that produces a thermomechanical loading on the fuel cladding. In conjunction with iodine expelled from the pellet, it can, in theory, lead to the failure of the cladding by Iodine Stress Corrosion Cracking (I-SCC).
The objective of this PhD is to study the phenomenology of I-SCC, in mechanical and chemical conditions as close as possible to the conditions seen by the PWR cladding in PCI (in terms of the oxygen and iodine partial pressures).
The PhD has three main parts. The first part will focus on the study of the effect of the stress on the I-SCC susceptibility of zirconium, at different partial pressures of iodine and oxygen. The tests will be simulated and analyzed using numerical models of the I-SCC process. The second part will focus on the effect of the temperature on I-SCC as a function of the stress, and the partial pressures of iodine and oxygen. The third part will focus on the effect of a thick zirconia layer, at the inner wall of the cladding, on the I-SCC susceptibility of the cladding.

Laboratory

Département de Recherche sur les Matériaux et la Physico-chimie pour les énergies bas carbone
Service d’Etudes des Matériaux Irradiés
Laboratoire de Comportement Mécanique des Matériaux Irradiés